The natural rubber manufacturing process begins with harvesting latex from rubber trees. Harvesting latex from rubber trees starts with scoring or cutting into the bark of the tree. Latex flows into a cup attached to the bottom of the cut in the tree. The latex material from many trees is accumulated in large tanks.
Characteristic
High Amonia
Total solid content
61.50 min (%)
Dry rubber content
60.00 min (%)
Amonia content (on total weight)
0.60 min (%)
Amonia content (on water phase)
1.60 min (%)
Non rubber content
2.00 min (%)
pH
11.00 max
Koh number
1.00 max
Volatile fatty acid number
0.05 max
Merchanical stability time
650 min (Secs)
Mangnesium content
60 max (ppm)
Colour of latex
White
Colour of film
Normal
Odour of latex
Sweet